Geobag dewatering · Laminated GCLs · Liner supply & technical supportGCL technical documents (10)
← All Kontain GCL products

GCL S37P · TECHNICAL DATA

Kontain GCL Standard 37 Polymer

Revision E · 7 November 2026

Standard 37 specifies ≥3,700 g/m² dry bentonite, a 100 g/m² woven carrier and polymer-modified sodium bentonite powder.

Needle-punched GCL without a PE laminate. Cover nonwoven ≥200 g/m². Carrier woven ≥100 g/m².

Minimum order: 3,000 m².

Technical data.

Production acceptance uses the specified grade and traceable roll and lot test records. Values are specified minimum and maximum acceptance limits. Dry bentonite mass covers the clay fraction, excluding polymer and geotextiles. Select each construction against its stated property schedule. Modified swell: 16 h after the final increment in ASTM D1193 reagent water (distilled/deionised) or 20,000 mg/L NaCl. Supplier reference values are ≥28 mL/2 g in tap water and ≥22 mL/2 g in 20,000 ppm salt water on the supplier basis. The stated reagent-water and NaCl conditions define acceptance targets. ASTM D5890-25 excludes polymers. Agree fluid-loss preparation. The Standard-grade fresh-water flux is a construction-specific acceptance target based on the same bentonite formulation as Heavy Duty. Specify ASTM D5887 acceptance testing for the selected construction and confinement.

PropertyMethod / basisValue
Dry bentonite massASTM D5993 plus formulation records≥3,700 g/m² excluding polymer
Cover nonwovenASTM D5261≥200 g/m²
Carrier wovenASTM D5261≥100 g/m²
Carrier nonwovenASTM D5261Not included
Total carrierComponent minima≥100 g/m²
Bentonite formulationControlled source and formulationPolymer-modified sodium bentonite powder
Tensile strength MD / CMDASTM D6768≥10 / ≥10 kN/m
Internal GCL peelASTM D6496≥360 N/m
CBR punctureEN ISO 12236≥1,600 N
Hydrated peak internal shearASTM D6243≥30 kPa at 10 kPa normal stress
Powder gradingValidated particle-size method≥80% passing 75 µm
Moisture contentASTM D5993≤13%
Fluid lossD5891-based modified-blend procedure≤18 mL
Modified swell in reagent waterASTM D5890-based modified method; 16 h after final increment≥28 mL/2 g
Modified swell in saline liquidASTM D5890-based modified method; 16 h after final increment; 20,000 mg/L NaCl≥22 mL/2 g
Core conductivity in fresh waterD5084 with agreed GCL setup≤5.0 × 10⁻¹¹ m/s
Fresh-water core index flux q10ASTM D5887; assumed from Heavy Duty; verify construction≤2.7 × 10⁻⁹ m³/m²/s
Core conductivity in 20,000 mg/L NaClD6766 within scope; identify adaptations≤1.0 × 10⁻¹⁰ m/s
Factory longitudinal edge overlapAccepted seam detail≥300 mm
End joints and field cuts on a baseAccessory bentonite treatment≥600 mm
Roll width and lengthCommon supply format5 × 30 m

Download the full TDS for the product construction and supply requirements.

Selection and installation.

Hydraulic limits apply to the GCL under agreed confinement, gradient, hydration, liquid and equilibrium criteria. Assess joint performance separately. Use ASTM D6766 within scope for chemicals and report adaptations. Specify durability, cycling and protection testing to suit the application. Consider polymer where higher drying resistance is sought during prolonged exposure, or lime-affected water, highly saline water or certain leachates may hydrate the clay instead of typical rainwater. Verify the actual liquid and formulation. Cover promptly; permanent exposed service requires separate design. Keep overlaps clean and in direct GCL contact under continuous confinement. Confirm factory edge treatment; use compatible accessory bentonite on untreated seams, ends and cuts. Slope end joints and repairs require project details. Agree roll dimensions and cores for the order.

Common rolls are 5 m × 30 m (150 m² gross). Custom dimensions, bentonite masses and plastic or steel cores are available by order. Confirm gross roll mass and clear core bore before lifting.

Provide the liner section, contact-soil grading and chemistry, liquid analysis, slope, loading, installation method and delivery requirements.

Read the installation guidance →